Sometimes, but not by sanding alone. If you live in Hempstead and the gaps between your floorboards bother you, refinishing can improve them when the boards are stable and the gaps are permanent. A pro can sand, push in a compatible filler, add wood slivers where the gaps are wide, and then seal everything under fresh finish. What refinishing cannot do is stop wood from moving with the seasons. Whether your gaps are fixable depends on why they opened in the first place.
We are Savera Wood Floor Refinishing, a veteran-owned, family-operated company serving Long Island. Below is how we think about gaps, what the research says, and how to decide between a screen and recoat, a repair, or a full sand when you are looking at hardwood floor refinishing in Hempstead.
TL;DR
- Refinishing can address gaps that are permanent and stable, using filler, spot repair or wood slivers, but it does not close gaps by itself.
- Many gaps are seasonal. They open when heated winter air dries the wood, and filling them then can backfire.
- Loose, cupped or water-damaged boards need to be stabilized before any finish goes down.
- A screen and recoat does not fix gaps. It refreshes a worn finish over sound boards, and it can sit alongside minor repairs.
- A proper in-person look at construction, moisture and board condition should come before anyone quotes you.
Table of Contents
- The short answer for Hempstead homeowners
- Why floorboards gap in the first place
- What refinishing can and cannot do about gaps
- Does every gap mean a full sand?
- When to wait before you refinish
- What a proper evaluation looks like
- Our perspective: diagnose first, then choose the lightest fix that works
- Older and historic Hempstead homes
- What you can do while you decide
- Costs and timing
- How Savera can help with floor gaps in Hempstead
- FAQ
- Ready to look at your floors?
- Sources
The short answer for Hempstead homeowners
Think of a gap as a symptom, not a finish problem. A finish sits on top of the wood. A gap is a space between two boards. Sanding makes the surface flat and ready for stain or sealer, but the space is still there unless something goes into it.
That is why a good contractor asks three questions before promising anything:
- Does the gap open and close with the seasons, or does it stay put all year?
- Are the boards tight to the subfloor, or do they move and creak underfoot?
- Is there any sign of moisture, such as cupping, staining or a damp slab or crawl space?
The answers sort your floor into one of three paths: a refresh, a repair plus refinish, or a full sand and refinish. We cover each below.
Why floorboards gap in the first place
Wood takes on and gives up moisture as the air around it changes. Ohio State University Extension explains that problems of dimensional change in wood products are directly tied to changes in moisture content. Boards shrink as they dry and swell as they absorb moisture.
Purdue Extension is the source for the figures used here: at 70°F, roughly 30% relative humidity corresponds to about 6% equilibrium moisture content, while roughly 70% corresponds to slightly less than 13%. That seven-point swing is enough to change board dimensions noticeably. A heated house in winter sits at the dry end of that range, which is why many gaps appear in January and shrink by summer.

On Long Island, that cycle is something most homeowners recognize: a hairline gap in the dining room in February that has nearly vanished by July. That is normal movement, not a defect.
Seasonal gaps versus permanent gaps
The distinction matters more than anything else in this article. According to National Wood Flooring Association (NWFA) guidance reported by Wood Floor Business, floors can be filled with wood filler or putty during sanding, but it is never a good idea to fill during winter months when seasonal gaps are present. The boards are at their smallest then. When humidity rises and they expand, filler can be pushed up out of the joint, and the board edges can be stressed.
In practice:
- Seasonal gaps close or narrow when the air gets humid. They usually call for humidity control and patience, not filler.
- Permanent gaps stay the same width year-round. They come from age, wear, shrinkage that has already happened, or installation issues, and they are the ones a refinish can help with.
When the cause is something else
Sometimes gaps are not about the season at all. A UMass Amherst building technology case study describes a floor that developed unsightly gaps within months of occupancy, with several boards looking significantly shrunken while large areas stayed tight. Moisture trapped in the construction was part of the story. In a case like that, filler and finish treat the look but not the cause.
That is also why we do not sell gap-closing as a cosmetic add-on before diagnosing the movement.
What refinishing can and cannot do about gaps
| Situation | Can refinishing help? | What it usually involves |
|---|---|---|
| Small, permanent gaps, stable boards | Yes | Sanding with compatible filler worked into the gaps, then finish |
| Larger permanent gaps | Yes, with repair | Wood slivers or inserts set into the gap, then sanding and finish |
| Seasonal gaps in dry months | Not by filling | Humidity control; reassess when the air is more humid |
| Loose or squeaky boards | Not until secured | Fasten or repair first, since loose floors do not hold filler |
| Cupped, buckled or water-damaged boards | Not first | Find the moisture source, dry gradually, repair or replace sections |
| Worn finish, no real gaps | Yes | Cleaning, then screen and recoat |
The repair methods above follow the NWFA sand and finish guidelines. They point to spot filler for larger cracks and holes, trowel filler on suitable square-edged floors, and wood slivers for bigger gaps. They also state that filler must be pushed into the gaps and voids, not just bridge across them, and that it needs to be compatible with the stain or finish. The same guidance warns that loose floors do not hold filler compounds, and that filler color can drift from light-sensitive wood as the floor ages.
That last point is worth a pause. A filler that matches today may look slightly different in three years, especially on species that change color with light. A good installer will tell you that up front rather than promise an invisible result. If you want to see how filler works in a typical home, our homeowner’s guide to using wood filler for floor gaps walks through it.
Does every gap mean a full sand?
No. This is the question we hear most from Hempstead homeowners who assume the answer is expensive and messy.
A worn finish over stable boards may be a candidate for cleaning, wax removal, minor repair and a screen and recoat. Deeper scratches, widespread discoloration, a failed finish, or repairs that need blending into raw wood generally call for more extensive sanding. The USDA Forest Products Laboratory treats repair and finish choices as condition-dependent, and we do too.
Screen and recoat: what it does for a gappy floor
A screen and recoat lightly abrades the existing finish and applies a fresh coat. It brings back sheen and protects the surface. It does not remove deep scratches and it does not close gaps. What it does do, on a floor with minor gaps that you plan to live with, is seal the top of the boards and make the floor easier to clean, because a finish in good shape is less likely to let dirt settle into the joints.
If your floor is a good candidate, our restore hardwood floors without sanding service uses dust-free methods and can often be completed with far less disruption than a full sand. If you are weighing the two approaches, our screen and recoat versus full sanding comparison lays out the trade-offs.
Full sanding: when it makes sense
If gaps are permanent, boards are stable, and the finish is also failing, a full sand lets the crew fill and repair in the raw wood, then stain and finish as one system. The filler is sanded flush and sealed under the same coats as the rest of the floor, which is the cleanest result. See our full hardwood floor sanding and refinishing page for what that involves, or the step-by-step refinishing process if you want to picture the days ahead.
When to wait before you refinish
Refinishing a floor that is still moving can hide a problem rather than cure it. Hold off if you see any of these:
- Cupping, where board edges sit higher than the centers
- Buckling, where boards lift off the subfloor
- Dark staining or a musty smell near gaps
- A known leak, a damp basement or crawl space, or a recent flood
University of Michigan guidance on repairing floors after water damage says wooden floors should be dried gradually and naturally, because sudden drying could cause cracking or splitting. It also says that damaged sections should be removed and repaired when buckling or unevenness remains. If water was involved, call a water restoration professional about the moisture source first. Refinishing comes after the floor is dry and flat.
If you rent out a property or are preparing to sell, the same logic applies. A fresh finish over wet or shifting boards will not survive a buyer’s inspection or a tenant’s first winter.
What a proper evaluation looks like
When we look at gaps in a Hempstead home, we are not just measuring widths. A thorough evaluation covers:
- Construction. Solid or engineered, board width, how it was installed. Engineered floors have a limited wear layer, which affects how much sanding is safe. Our engineered hardwood refinishing page explains this.
- Stability. Walking the floor to find loose, squeaky or damaged boards.
- Moisture and humidity. What the indoor conditions are, and whether anything suggests an active moisture source.
- Season. Whether the gaps are likely seasonal, so nobody fills a joint at its widest or narrowest.
- Finish condition. Whether it is worn, waxed, peeling or intact, which decides between a recoat and a sand.
The 2026 NWFA installation guidelines reinforce that wood flooring performance depends on proper installation, acclimation and maintenance, not on finish alone. That is the current reference for how wood and its environment interact.
Our perspective: diagnose first, then choose the lightest fix that works
We get a lot of calls that start with, “Can you just fill these gaps and refinish?” Our honest answer is that it depends, and we would rather tell you that than sell you a treatment that fails by next winter.
Here is what guides us. A floor is a living material. If a gap opens and closes with the seasons, the right fix is usually to leave it alone and manage indoor humidity. If a gap is permanent, filling or setting a sliver is a sound repair, and doing it during a sand gives the cleanest blend. And if the floor is in decent shape with only a tired finish, you may not need to sand at all.
We built our process around that last idea. Our dust-free sanding system uses HEPA-filtered vacuums and sectional plastic protection, so the work stays contained. We use low-VOC, odor-free water-based finishes that are safer for families and pets. And where a floor is a fit, our UV-curable finish cures instantly, so in many cases furniture can go back the same day. For a family that has been tiptoeing around a project for days, that matters.
We also specialize in older floors that may no longer be ideal candidates for aggressive sanding. Every sand removes wood, and some floors have only so much left to give. Sometimes the best thing we can do is breathe new life into the wood with a careful clean, a repair and a fresh coat rather than taking it down to raw.
— Savera
Older and historic Hempstead homes
If your home has original floors, gaps may be part of its character. Historic boards were often narrower, dried over decades, and shrank. The National Park Service preservation guidance says condition should be weighed carefully, asking whether flooring is repairable or deteriorated beyond repair. Repair is preferred when the material can be repaired, and a replacement should match the historic material and its visual characteristics.
For a damaged board or a stubborn wide gap, a matched wood insert, often called a Dutchman, can be the least invasive route. The GSA’s procedure for Dutchman repair describes removing the damaged portion with a hammer and chisel, beveling the edges of the cavity, and fitting a matched piece. That is a hands-on, careful job, which is the point: a few repairs can save a whole floor from replacement.
If you have a historic floor, tell us when you call. We would rather start with the gentlest option and only sand more if the floor needs it.

What you can do while you decide
You do not have to settle on a plan today. A few practical steps help:
- Note when the gaps are widest. Take a photo with a coin for scale in winter, and again in summer. That one comparison tells us a lot.
- Watch indoor humidity. A simple hygrometer shows how dry the house gets in heating season.
- Skip store-bought fillers in winter. If gaps are seasonal, a filler job now can pop out later.
- Check for moisture. Look near exterior walls, under sinks and above damp basements.
- Keep furniture pads on. Scratches in an open gap are harder to repair than scratches on a flat board.
Costs and timing
We do not publish a price for gap repair, and there is no authoritative universal figure to quote. Cost and downtime depend on floor area, access, board condition, the amount of repair, the finish system and whether the job is a screen and recoat or a complete restoration. We would rather look at your floor and give you a straight number than guess.
One published figure on our site: custom stain is listed at $1 per square foot. Staining is relevant if a repair means blending new wood into the old. Our staining and color change page has more on how that works.
How Savera can help with floor gaps in Hempstead
If you want a straight answer on your own floor, we can look at the boards, the finish and the gaps, and recommend the lightest approach that will last. Depending on what we find, that could be:
- A screen and recoat or restoration without sanding for sound floors with a tired finish
- Hardwood floor repair, sanding and refinishing when gaps, damaged boards or deeper wear need attention
- A UV-cured finish when you need the floor back in use quickly, such as a rental turnover or a busy household
You can also see our local page for hardwood floor refinishing in West Hempstead.
FAQ
Will sanding close the gaps between my floorboards?
No. Sanding smooths and levels the surface but does not move the boards together. Gaps are closed by filling them with a compatible filler or by setting wood slivers in, and that is done as part of the sanding stage.
Should I fill gaps in the winter?
Generally not if the gaps are seasonal. NWFA guidance reported by Wood Floor Business advises against filling during winter months when seasonal gaps are present, since the boards are at their smallest and filler can be pushed out when they expand. A professional can help tell seasonal gaps from permanent ones.
Can a screen and recoat hide gaps?
It will not close them, though the fresh coat seals the surface and improves the floor’s look. If gaps are your main concern, a repair and refinish is the better path. A screen and recoat is for floors with sound boards and a worn finish.
Are large gaps repairable?
Often, yes, if the boards are stable. For larger gaps, NWFA guidance describes wood slivers, and for damaged boards a matched insert may work. If the floor is loose, cupped or water damaged, the cause has to be dealt with first.
How do I know if my Hempstead floor needs a full sand?
A full sand is generally needed when the finish has failed, scratches are deep, discoloration is widespread, or repairs have to be blended into raw wood. If the boards are stable and the finish is only worn, a lighter option may be enough. An in-person look is the surest way to tell.
Ready to look at your floors?
If gaps have you wondering what your floors need, we are happy to take a look and give you an honest recommendation for your Hempstead home. Call Savera Wood Floor Refinishing at 631-866-1972 or visit saverawoodfloorrefinishing.com to book your appointment.
Sources
- Understanding Dimensional Changes In Wood Products, Ohioline
- FNR-37, Purdue Extension
- Q&As: Popping Putty, Extra Poly Coats & Installing HDF Floors, Wood Floor Business
- Common Failures in Wood Structures, UMass Amherst
- Wood Flooring Sand and Finish Guidelines, NWFA
- USDA Forest Products Laboratory, EX136
- Repairing Floors from Water Damage to Prevent Mold Growth, University of Michigan
- Wood Flooring Installation Guidelines, NWFA 2026